Holes too small or parts don't fit
Holes come out smaller than designed, or parts that should fit together are too tight. Plastic shrinks and spreads a little as it prints, so some allowance is normal, but extra plastic from over-extrusion makes it worse.
Fixes, in the order to try them:
- Run the slicer's flow calibration and set the flow ratio from the result.
- Use the slicer's elephant foot compensation, often 0.1 to 0.2 mm, and lower the bed temperature a few degrees if the bulge remains.
- Use hole horizontal expansion, sometimes called XY hole compensation, to enlarge holes, starting around 0.1 mm.
- Design in clearance, leaving a gap of about 0.2 mm between mating surfaces for a sliding fit and 0.4 mm for a loose fit.
- Export models at a finer resolution so circles stay round.
- Set the material's shrinkage compensation for ABS, ASA and nylon after measuring a test part.
- Drill or ream critical holes to size after printing when you need an exact fit.