First layer won't stick
The first layer peels up, drags around behind the nozzle, or the print comes loose early. It is almost always the nozzle sitting too far from the bed, or a bed surface with oil or dust on it.
Fixes, in the order to try them:
- Wash the bed with dish soap and warm water or wipe it with isopropyl alcohol, then don't touch it.
- Re-run bed leveling with the bed hot, since beds change shape slightly as they heat up.
- Lower the Z offset in small steps, about 0.02 mm at a time, until lines are slightly squished and touching.
- Slow the first layer to about 20 to 30 mm/s.
- Print the first layer 5 to 10°C hotter than the rest of the print.
- Make sure the part cooling fan is off or low for the first layer.
- Use a glue stick or bed adhesive on glass or smooth surfaces.
- Replace a worn PEI sheet, or flip it if it is double-sided, when shiny worn patches no longer hold.