Layers splitting or cracking
Your part cracks or splits along the lines between layers, often on tall prints or when you flex it. The layers didn't fuse well, usually because the plastic cooled too fast or was printed too cold.
Fixes, in the order to try them:
- Raise the nozzle temperature 5 to 10°C, staying inside the label's range.
- Turn part cooling down to 0 to 20% for ABS and ASA, and keep it low for PC as well.
- Print ABS, ASA and PC in an enclosure, and let the bed heat for 10 to 15 minutes first so the air inside warms up.
- Block drafts from windows, fans and air vents, and try the slicer's draft shield option on open printers.
- Slow down or lower the slicer's maximum volumetric speed, which limits how much plastic per second the hotend must melt.
- Keep layer height under about 75% of the nozzle diameter, for example 0.3 mm or less on a 0.4 mm nozzle.
- Dry the filament if it pops or bubbles while printing.
- Orient the part so the main load runs along the layers instead of pulling them apart.