Rough or bumpy top surfaces
The top of your print is lumpy, ridged or full of small gaps instead of smooth and flat. Usually there aren't enough top layers to cover the infill, or the printer is laying down too much or too little plastic.
Fixes, in the order to try them:
- Use at least 4 to 6 top layers, or about 0.8 to 1 mm of total top thickness.
- Raise infill to 15 to 20%, or use gyroid infill, so the top layers have more to rest on.
- Run the slicer's flow calibration and set the flow ratio from the result.
- Slow down the top surface speed and use full part cooling on top layers for PLA.
- Choose a monotonic top pattern, which lays every line in the same direction for a more even finish.
- Turn on ironing, a final slow pass with the hot nozzle, to smooth flat top surfaces.
- Dry the filament if you see bubbles or hear popping.