Under-extrusion and gaps
The printer isn't pushing out enough plastic, so walls look thin and gappy and top surfaces have holes. Common reasons are a partial clog, printing too fast for the nozzle temperature, or filament that can't feed freely.
Fixes, in the order to try them:
- Make sure the spool turns freely and the tube from spool to extruder isn't kinked.
- Raise the nozzle temperature 5 to 10°C, or lower the print speed.
- Clear a partial clog with a cold pull, or replace the nozzle (heat it first and follow your printer's instructions).
- Clean ground-up plastic out of the extruder gears with a small brush.
- Dry the filament if it pops or crackles while printing.
- Run the flow calibration in your slicer, or calibrate e-steps on older printers.
- Lower the max volumetric speed (how much plastic per second the hotend can melt) in the filament profile if gaps only appear at speed.