Warping and lifting corners
The corners of the print curl up off the bed, often partway through the print. Plastic shrinks as it cools, and if the upper layers cool faster than the bottom or the part isn't stuck well, the edges get pulled up.
Fixes, in the order to try them:
- Wash the bed with dish soap and warm water, rinse, dry, and avoid touching it afterward.
- Raise the bed temperature toward the top of the label range, about 60°C for PLA, 80°C for PETG, and 100 to 110°C for ABS and ASA.
- Block drafts, and use an enclosure for ABS, ASA, nylon and PC.
- Add a brim (a thin flat border attached to the part) of 5 to 10 mm, or small discs on the corners.
- Turn the part cooling fan off for the first few layers, and keep it low for ABS and ASA.
- Lower the Z offset slightly so the first layer is pressed firmly into the bed.
- Use a glue stick or a bed adhesive made for that material on smooth or glass surfaces.
- Round off sharp corners in the model, or split very large flat parts into smaller pieces.