Wet filament (popping, bubbles, rough surface)
Your nozzle pops or crackles and prints come out rough, stringy or weak. Most filament slowly soaks up moisture from the air, and that water boils into steam as it passes through the hot nozzle.
Fixes, in the order to try them:
- Dry the spool in a filament dryer, usually for 4 to 8 hours, at the temperature on the label or in the material notes below.
- Use these drying starting points: PLA 45 to 55°C, PETG 60 to 65°C, TPU 50 to 55°C, ABS and ASA 70 to 80°C, nylon 70 to 80°C.
- Keep PLA below about 55°C while drying, because it softens and the coils can fuse together.
- Don't dry filament in a kitchen oven, since many overshoot at low settings and can soften the spool or the filament.
- After drying, print right away or move the spool into a sealed box with fresh desiccant.
- Print nylon and TPU straight from a running dryer box so they stay dry during long prints.
- If stringing remains after drying, tune temperature and retraction next, since those changes only work on dry filament.